Electroless Plating of PZT Tubes Issue date Feb. 2009
A conductive layer is often required on PZT (lead zirconium titanate) ceramic tube material, to allow soldering. This technical note is using the standard Smart Material tube with 1.1 mm OD and 0.5 mm ID and about 10cm long. Plating is required inside the bore |
100 kB |